Customization: | Available |
---|---|
Type: | Rolling Wire |
Material: | Tin |
Still deciding? Get samples of US$ 0.00/30G
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
1. Features:
When applied in the wave soldering ovens, the common solder bar can often produce a large amount of solder splash or unmelted solder.
So far, our Sn63Pb37 no-clean tin lead solder wire and solder bar has been exported to United States, Russia, Germany, India, and Brazil, among other countries. We are also looking for agents on a global
2. Specification:
No. |
Item |
SPEC |
1 |
Components |
Sn63Pb37 |
2 |
Flux Content % |
2.0 |
3 |
Flux continuity |
good fluidness |
4 |
Halide Content (Wt%) |
<0.5 |
5 |
Copper Plate Corrosion |
Pass |
6 |
Copper Mirror Corrosion |
Pass |
7 |
Insulated Resistance (Ω) |
10 >1X10 |
8 |
Water-soluble resistors (Ω.cm) |
10 >1X10 |
9 |
Extend rate % |
>90 |
10 |
Residuum |
Pass |
11 |
Diameter (mm) |
Φ0.2-3.0mm |
12 |
Packing |
10reel/carton, 10kg/carton |
Components |
Impurity Content % |
|||||||||||
Norm |
Sn |
Pb |
Sb |
Ag |
Cu |
Fe |
Zn |
Bi |
Al |
As |
Ni |
Cd |
63±0.8 |
Margin |
≤0.10% |
≤0.02% |
0.1% |
≤0.02% |
≤0.001% |
≤0.10% |
≤0.001% |
≤0.03% |
≤0.01% |
<0.01% |
|
Results |
62.5 |
Margin |
0.032 |
0.0002 |
0.0057 |
0.002 |
0.0015 |
0.006 |
0.0024 |
0.0021 |
0.0032 |
0.0001 |